Low-gloss interior trim, no paint line
OEM asked for 2.5 GU at 60 degrees on a moulded part. Painted ABS was failing the scratch test after 6 months in the field.
2.1 GU, paint line removed
Home / Solutions
APPLICATION CASES · 8 ON FILE
A grade name answers what it is. These cases record the constraint that was failing, and the material that went in.
OEM asked for 2.5 GU at 60 degrees on a moulded part. Painted ABS was failing the scratch test after 6 months in the field.
2.1 GU, paint line removed
Crazing around the detergent drawer after 200 hours of splash testing. The old grade was a cheap GPPS blend.
500 h wipe, no crazing, higher impact
Halogen-free FR PC/ABS was passing V-0 but leaving a white bloom on the housing after 3 weeks in a hot warehouse.
V-0 at 1.5 mm, no bloom
The incumbent PP yellowed after 25 kGy. The customer needed a lower colour shift and ISO 10993-1 on file.
Lower colour shift after 25 kGy
The shell was cracking at the battery latch in a 1.8 m cold drop test. Unfilled PA6 was too notch-sensitive.
1.8 m drop pass
The customer was replacing impellers every 9 months in mildly alkaline water. Both candidates ran for a season.
Longer wear life in alkaline water
Filling a 0.55 mm rib on a short cycle. Standard impact copolymer was short-shotting at the gate.
0.55 mm fill, shorter cycle
A stamped steel bracket held at 120 C continuous. The first metal swap still weighed too much.
Lighter part, 120 C continuous